| Material Data Sheet | | | | | | | | Weight(GMS) | 2883 | | | | Stress rate (KN/min) | 30 | | | | Diameter (mm) | 100 | | | | Height(mm) | 150 | | | | Maximum Load (KN) | 527 | | | | Measure compressive strength (N/mm sq) | 67.09 |
| | | Model of failure | Axial | | | | Water absorption (%) | |
| | | | | | | Chemical Analysis (%) | | | | | | | | | Silica | 80.31 | | | | Alumina | 8.31 | | | | Iron oxide | .40 | | | | Lime | - | | | | Magnesia | .43 | | | | Potassium oxide | .20 | | | | Sodium oxide | .88 |
| | | | | | | | Based upon samples of 40-20mm stone | | |
|